German Rochling Gray Durostone CFR767


CFR767-3


The combination of processing cycles in high temperature environments combined with aggressive fluxes can cause degradation of standard Durostone grades.

The solution is Durostone CFR767, which is specially formulated for aggressive fluxes and high temperature process configurations.

The resin used to produce Durostone CFR767 can withstand temperatures up to 300°C. When the solder bath temperature exceeds 265°C and the bottom PCB preheat exceeds 140°C, Durostone CFR767 should be used instead of the standard grade.

Durostone CFR767 has excellent flux resistance. When fluxes containing halides or dicarboxylic acids are used in high-volume production, the lifetime of standard grade materials is reduced, so Durostone CFR767 is the ideal solution.

Paqij bûn

Author:

Ms. Tina

Phone/WhatsApp:

8618680371609

Products
Nûçeya Kompaniyê
Blog News
What Is PEEK Ball ?

November 13, 2024

PVDF Application Areas

November 03, 2024

You may also like
Related Categories

Ji bo vê pargîdaneyê bişînin

Mijar:
Destpê bikin:
Email:
Agah:

Your message must be betwwen 20-8000 characters

Paqij bûn

Author:

Ms. Tina

Phone/WhatsApp:

8618680371609

Products
Nûçeya Kompaniyê
Blog News
What Is PEEK Ball ?

November 13, 2024

PVDF Application Areas

November 03, 2024

Em ê bi we re bi navgîniya xwe re têkilî daynin

Agahdariya bêtir dagirtin da ku bi we re zûtir têkiliyê bi we re têkevin

Daxuyaniya nepenîtiyê: Parastina we ji me re pir girîng e. Pargîdaniya me soz nedan ku agahdariya kesane ya we ji her pêşangehên we yên eşkere eşkere bike.

Şandin